Slab & Flatwork

4 guides with the numbers shown, not just the conclusions.

Slab work starts with three decisions: the right thickness, the exact volume, and the right reinforcement for the load. These guides cover each decision in order, with the numbers and rules a homeowner or contractor needs on any site. You will find thickness rules by use, a full step by step volume walkthrough, and clear reinforcement options for each load and use.

One guide compares welded wire mesh with rebar and explains where each belongs in patios, driveways, and garage slabs. Another guide sizes rebar by diameter and sets typical grid spacing for slabs that support vehicles and heavy equipment. Correct thickness and correct steel placement prevent cracks, curling, and settling, so plan both carefully before you order any concrete.

Plan a Slab in This Order

Each decision sets up the next one. Thickness comes from the load, volume comes from the thickness, and steel comes from both. Pricing before you settle thickness means doing the budget twice.

What Extra Thickness Really Adds

Going from 4 to 6 in adds 0.62 yd³ for every 100 square feet. At $175 per yard that is about $108 in concrete, while the base preparation and finishing area stay the same. These figures are exact volumes before waste.

Thicknessyd³ per 100 ft²Weight per ft²Typical use
4 in1.2350 lbPatios, paths, light sheds
5 in1.5462.5 lbCar driveways, garages
6 in1.8575 lbHeavier vehicles, RV pads
8 in2.47100 lbHeavy equipment, by design

Problems That Thickness Cannot Fix

A slab is only as steady as the ground under it. Soft spots, buried topsoil, and loose fill settle unevenly, and the slab bridges the gap until it cracks. Remove organic soil, compact in layers, and finish with a level gravel base. The gravel calculator gives base quantities.

Shrinkage is the other cause. All concrete shrinks as it dries, so expect cracks somewhere. Control joints cut about a quarter of the slab depth, 1 in deep in a 4 in slab, put the crack in a straight line where you want it. Steel holds that crack closed. It does not prevent it.

The third is drying too fast. Hot, windy weather pulls water off the surface before the concrete gains strength. Keep it damp or covered for about seven days, and keep vehicles off until it has had time to harden.